► A conduction-cooled HTS magnet for SPMS was fabricated and tested. ► Split-pair winding configuration was used for obtaining magnetic field uniformity. ► Room temperature bore was 38mm (L)×134mm (W)×360mm (D) in dimension. ► The magnetic field uniformity was achieved lower than 1%. ► Also, Such HTS magnet could be operated to generate 3T for 7h.
A conduction-cooled high temperature superconducting (HTS) magnet for the SPMS was fabricated and tested. To achieve an adequate uniformity of background magnetic field, a split-pair winding configuration is used. Room temperature bore of this magnet was 38mm (length)×134mm (width)×360mm (depth) in dimension. The magnetic field uniformity of HTS magnet was achieved lower than 1% within the virtual sample region 15mm (width)×100mm (depth). Also, this HTS magnet could be operated to generate 3T for 7h.