Coprecipitated iron-containing catalysts (Fe-Al 2O 3, Fe-Co-Al 2O 3, Fe-Ni-Al 2O 3) for methane decomposition at moderate temperatures : I. Genesis of calcined and reduced catalysts
Ist Teil von
  • Applied catalysis. A, General, 2004-08, Vol.268 (1), p.127-138
Ort / Verlag
Amsterdam: Elsevier B.V
Erscheinungsjahr
2004
Quelle
Access via ScienceDirect (Elsevier)
Beschreibungen/Notizen
  • Genesis of the composition and structure of the active component of coprecipitated iron containing catalysts (Fe-Al 2O 3, Fe-Co-Al 2O 3, Fe-Ni-Al 2O 3) with high metal loadings (>50 wt.%) for methane decomposition at moderate temperatures (600–650 °C) has been investigated by XRD, EXAFS, radial electron density distribution (REDD), TEM, FTIR and Mössbauer spectroscopy. The main stages of the catalyst genesis during drying, thermal decomposition and reduction have been studied. For bimetallic systems (Fe-Co-Al 2O 3, Fe-Ni-Al 2O 3) intermediate spinel phases with a composition (M II, Fe) 3O 4 (M=Co, Ni) have been shown to form during heat treatment and reduction. This leads to a decrease of the reduction temperature for iron oxides. Reduced bimetallic catalysts (Fe-Co-Al 2O 3, Fe-Ni-Al 2O 3) are composed of alloys. The structure and parameters of their crystal lattices depend on the type and concentration of the added metal. Alumina has been shown to behave as a structural promoter. A model of the reduced catalysts consisting of highly dispersed (20–50 nm) metal and alumina particles with a spinel phase at their interface has been suggested.
Sprache
Englisch; Russisch
Identifikatoren
ISSN: 0926-860X
eISSN: 1873-3875
DOI: 10.1016/j.apcata.2004.03.045
Titel-ID: cdi_pascalfrancis_primary_15815092

Weiterführende Literatur

Empfehlungen zum selben Thema automatisch vorgeschlagen von bX